Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.15 g/cm³ Show Material materials with Dichte of 7.15 g/cm³ | Typical for Grey Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive yield strength | 20.0 °C | 860 - 1100 MPa Show Material materials with Compressive yield strength of 860 - 1100 MPa | |
Dehnung | 20.0 °C | 1 % Show Material materials with Dehnung of 1 % | |
Elastizitätsmodul | 23.0 °C | 92.4 GPa Show Material materials with Elastizitätsmodul of 92.4 GPa | Typical for Grey Cast Iron |
Härte, Brinell | 20.0 °C | 150 - 250 [-] Show Material materials with Härte, Brinell of 150 - 250 [-] | |
Poissonzahl | 23.0 °C | 0.21 [-] Show Material materials with Poissonzahl of 0.21 [-] | Typical for Grey Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Zugfestigkeit | 20.0 °C | 190 - 240 MPa Show Material materials with Zugfestigkeit of 190 - 240 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.5E-5 1/K | Typical for Grey Cast Iron |
Schmelzpunkt | 1127 - 1204 °C Show Material materials with Schmelzpunkt of 1127 - 1204 °C | Typical for Grey Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Grey Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 20 - 80 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 20 - 80 W/(m·K) | Typical for Grey Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 2.5 - 3.5 % Show Material materials with Chrom of 2.5 - 3.5 % |
Kohlenstoff | 3 % Show Material materials with Kohlenstoff of 3 % |
Kupfer | 5.5 - 7.5 % Show Material materials with Kupfer of 5.5 - 7.5 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 13.5 - 17.5 % Show Material materials with Nickel of 13.5 - 17.5 % |
Silizium | 1 - 2.8 % Show Material materials with Silizium of 1 - 2.8 % |