Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.15 g/cm³ Show Material materials with Dichte of 7.15 g/cm³ | Typical for Ductile (Nodular) Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 7 % Show Material materials with Dehnung of 7 % | |
Elastizitätsmodul | 23.0 °C | 165 - 180 GPa Show Material materials with Elastizitätsmodul of 165 - 180 GPa | Typical for Ductile (Nodular) Cast Iron |
Härte, Brinell | 20.0 °C | 140 - 200 [-] Show Material materials with Härte, Brinell of 140 - 200 [-] | |
Poissonzahl | 23.0 °C | 0.26 - 0.31 [-] Show Material materials with Poissonzahl of 0.26 - 0.31 [-] | Typical for Ductile (Nodular) Cast Iron |
Schubmodule | 23.0 °C | 63 - 66 GPa Show Material materials with Schubmodule of 63 - 66 GPa | Typical for Ductile (Nodular) Cast Iron |
Streckgrenze | 20.0 °C | 210 - 250 MPa Show Material materials with Streckgrenze of 210 - 250 MPa | |
Zugfestigkeit | 20.0 °C | 370 - 480 MPa Show Material materials with Zugfestigkeit of 370 - 480 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.6E-5 1/K | Typical for Ductile (Nodular) Cast Iron |
Schmelzpunkt | 1150 - 1200 °C Show Material materials with Schmelzpunkt of 1150 - 1200 °C | Typical for Ductile (Nodular) Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 502 J/(kg·K) | Typical for Ductile (Nodular) Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 13 - 42 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 - 42 W/(m·K) | Typical for Ductile (Nodular) Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 1 - 2.5 % Show Material materials with Chrom of 1 - 2.5 % |
Kohlenstoff | 3 % Show Material materials with Kohlenstoff of 3 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 18 - 22 % Show Material materials with Nickel of 18 - 22 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Silizium | 1.5 - 3 % Show Material materials with Silizium of 1.5 - 3 % |