Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Dichte of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 7 % Show Material materials with Dehnung of 7 % | |
Elastizitätsmodul | 23.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa | Typical for Cast Iron |
Härte, Brinell | 20.0 °C | 150 - 255 [-] Show Material materials with Härte, Brinell of 150 - 255 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Streckgrenze | 20.0 °C | 210 - 260 MPa Show Material materials with Streckgrenze of 210 - 260 MPa | |
Zugfestigkeit | 20.0 °C | 390 - 500 MPa Show Material materials with Zugfestigkeit of 390 - 500 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 2.5 - 3.5 % Show Material materials with Chrom of 2.5 - 3.5 % |
Kohlenstoff | 3 % Show Material materials with Kohlenstoff of 3 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 18 - 22 % Show Material materials with Nickel of 18 - 22 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Silizium | 1.5 - 3 % Show Material materials with Silizium of 1.5 - 3 % |