Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.4 g/cm³ Show Material materials with Dichte of 7.4 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 165 - 180 GPa Show Material materials with Elastizitätsmodul of 165 - 180 GPa | |
Härte, Vickers | 20.0 °C | 300 [-] Show Material materials with Härte, Vickers of 300 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 2.8 - 3.5 % Show Material materials with Kohlenstoff of 2.8 - 3.5 % |
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % |
Molybdän | 0.5 - 0.8 % Show Material materials with Molybdän of 0.5 - 0.8 % |
Nickel | 1.5 - 4.5 % Show Material materials with Nickel of 1.5 - 4.5 % |
Silizium | 2 - 2.6 % Show Material materials with Silizium of 2 - 2.6 % |