Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 17 % Show Material materials with Dehnung of 17 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 440 - 500 MPa Show Material materials with Streckgrenze of 440 - 500 MPa | |
Streckgrenze Rp 0,2 | 50.0 °C | 430 - 490 MPa Show Material materials with Streckgrenze Rp 0,2 of 430 - 490 MPa | |
100.0 °C | 410 - 470 MPa Show Material materials with Streckgrenze Rp 0,2 of 410 - 470 MPa | ||
150.0 °C | 390 - 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 390 - 450 MPa | ||
200.0 °C | 360 - 420 MPa Show Material materials with Streckgrenze Rp 0,2 of 360 - 420 MPa | ||
250.0 °C | 340 - 400 MPa Show Material materials with Streckgrenze Rp 0,2 of 340 - 400 MPa | ||
300.0 °C | 320 - 380 MPa Show Material materials with Streckgrenze Rp 0,2 of 320 - 380 MPa | ||
Zugfestigkeit | 20.0 °C | 540 - 770 MPa Show Material materials with Zugfestigkeit of 540 - 770 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.018 % Show Material materials with Aluminium of 0.018 % |
Bor | 5E-3 % Show Material materials with Bor of 5E-3 % |
Chrom | 1 % Show Material materials with Chrom of 1 % |
Kohlenstoff | 0.18 % Show Material materials with Kohlenstoff of 0.18 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1.7 % Show Material materials with Mangan of 1.7 % |
Molybdän | 0.7 % Show Material materials with Molybdän of 0.7 % |
Nickel | 1.5 % Show Material materials with Nickel of 1.5 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 - 0.015 % Show Material materials with Schwefel of 0.01 - 0.015 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % |
Zirkonium | 0.15 % Show Material materials with Zirkonium of 0.15 % |