Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.15 g/cm³ Show Material materials with Dichte of 7.15 g/cm³ | Typical for Grey Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 92.4 GPa Show Material materials with Elastizitätsmodul of 92.4 GPa | Typical for Grey Cast Iron |
Härte, Brinell | 20.0 °C | 105 - 175 [-] Show Material materials with Härte, Brinell of 105 - 175 [-] | |
Poissonzahl | 23.0 °C | 0.21 [-] Show Material materials with Poissonzahl of 0.21 [-] | Typical for Grey Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.5E-5 1/K | Typical for Grey Cast Iron |
Schmelzpunkt | 1127 - 1204 °C Show Material materials with Schmelzpunkt of 1127 - 1204 °C | Typical for Grey Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Grey Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 20 - 80 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 20 - 80 W/(m·K) | Typical for Grey Cast Iron |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting |