Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.1 g/cm³ Show Material materials with Dichte of 7.1 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive yield strength | 20.0 °C | 700 MPa Show Material materials with Compressive yield strength of 700 MPa | |
Dehnung | 20.0 °C | 18 % Show Material materials with Dehnung of 18 % | |
Elastizitätsmodul | 20.0 °C | 169 GPa Show Material materials with Elastizitätsmodul of 169 GPa | |
Poissonzahl | 20.0 °C | 0.28 [-] Show Material materials with Poissonzahl of 0.28 [-] | |
Scherfestigkeit | 20.0 °C | 360 MPa Show Material materials with Scherfestigkeit of 360 MPa | |
Schubmodule | 23.0 °C | 63 - 66 GPa Show Material materials with Schubmodule of 63 - 66 GPa | Typical for Ductile (Nodular) Cast Iron |
Streckgrenze Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa | |
Zugfestigkeit | 20.0 °C | 400 MPa Show Material materials with Zugfestigkeit of 400 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 400.0 °C | 1.25E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.25E-5 1/K | |
Schmelzpunkt | 1150 - 1200 °C Show Material materials with Schmelzpunkt of 1150 - 1200 °C | Typical for Ductile (Nodular) Cast Iron | |
Spezifische Wärmekapazität | 500.0 °C | 515 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 515 J/(kg·K) | |
Wärmeleitfähigkeit | 300.0 °C | 36.2 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36.2 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 5E-7 Ω·m Show Material materials with spezifischer Widerstand of 5E-7 Ω·m |