Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.15 g/cm³ Show Material materials with Dichte of 7.15 g/cm³ | Typical for Ductile (Nodular) Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 18 % Show Material materials with Dehnung of 18 % | |
Elastizitätsmodul | 23.0 °C | 165 - 180 GPa Show Material materials with Elastizitätsmodul of 165 - 180 GPa | Typical for Ductile (Nodular) Cast Iron |
Poissonzahl | 23.0 °C | 0.26 - 0.31 [-] Show Material materials with Poissonzahl of 0.26 - 0.31 [-] | Typical for Ductile (Nodular) Cast Iron |
Schubmodule | 23.0 °C | 63 - 66 GPa Show Material materials with Schubmodule of 63 - 66 GPa | Typical for Ductile (Nodular) Cast Iron |
Streckgrenze Rp 0,2 | 20.0 °C | 240 MPa Show Material materials with Streckgrenze Rp 0,2 of 240 MPa | |
Zugfestigkeit | 20.0 °C | 400 MPa Show Material materials with Zugfestigkeit of 400 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.6E-5 1/K | Typical for Ductile (Nodular) Cast Iron |
Schmelzpunkt | 1150 - 1200 °C Show Material materials with Schmelzpunkt of 1150 - 1200 °C | Typical for Ductile (Nodular) Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 502 J/(kg·K) | Typical for Ductile (Nodular) Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 13 - 42 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 - 42 W/(m·K) | Typical for Ductile (Nodular) Cast Iron |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 3.5 - 3.8 % Show Material materials with Kohlenstoff of 3.5 - 3.8 % |
Magnesium | 0.06 - 0.12 % Show Material materials with Magnesium of 0.06 - 0.12 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 2 - 3 % Show Material materials with Silizium of 2 - 3 % |