Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 38 % Show Material materials with Dehnung A50 of 38 % | |
Dehnung A80 | 23.0 °C | 38 % Show Material materials with Dehnung A80 of 38 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 120 MPa Show Material materials with Streckgrenze of 120 MPa | |
Zugfestigkeit | 23.0 °C | 350 MPa Show Material materials with Zugfestigkeit of 350 MPa |