Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.72 - 2.73 g/cm³ Show Material materials with Dichte of 2.72 - 2.73 g/cm³ | Typical for Wrought 3000 Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | H22 | JIS H4001 | Sheet | |
Elastizitätsmodul | 69.5 - 70.0 GPa Show Material materials with Elastizitätsmodul of 69.5 - 70.0 GPa | Typical for Wrought 3000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | |||
Schubmodule | 25.0 - 26.0 GPa Show Material materials with Schubmodule of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium | |||
Streckgrenze | 118.0 MPa Show Material materials with Streckgrenze of 118.0 MPa | H22 | JIS H4001 | Sheet | |
Zugfestigkeit | 137.0 MPa Show Material materials with Zugfestigkeit of 137.0 MPa | H22 | JIS H4001 | Sheet |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium |
Schmelzpunkt | 629.0 - 654.0 °C Show Material materials with Schmelzpunkt of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Spezifische Wärmekapazität | 893.0 - 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium |
Wärmeleitfähigkeit | 154.0 - 193.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 154.0 - 193.0 W/(m·K) | Typical for Wrought 3000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Technological properties
Property | ||
---|---|---|
Processing history | H22 | |
Workability | Good workability. |