Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1 - 1.8 % Show Material materials with Aluminium of 1 - 1.8 % |
Chrom | 18 - 21 % Show Material materials with Chrom of 18 - 21 % |
Eisen | 1.5 % Show Material materials with Eisen of 1.5 % |
Kohlenstoff | 0.04 - 0.1 % Show Material materials with Kohlenstoff of 0.04 - 0.1 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 1.8 - 2.7 % Show Material materials with Titan of 1.8 - 2.7 % |
Technological properties
Property | ||
---|---|---|
Processing history | ageing treatment after solution treatment |