Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.2 - 7.34 g/cm³ Show Material materials with Dichte of 7.2 - 7.34 g/cm³ | Typical for Malleable Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 6 % Show Material materials with Dehnung A5 of 6 % | |
Elastizitätsmodul | 23.0 °C | 165 - 180 GPa Show Material materials with Elastizitätsmodul of 165 - 180 GPa | Typical for Malleable Cast Iron |
Härte, Brinell | 23.0 °C | 149 - 207 [-] Show Material materials with Härte, Brinell of 149 - 207 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Malleable Cast Iron |
Schubmodule | 23.0 °C | 64 GPa Show Material materials with Schubmodule of 64 GPa | Typical for Malleable Cast Iron |
Streckgrenze Rp 0,2 | 23.0 °C | 265 MPa Show Material materials with Streckgrenze Rp 0,2 of 265 MPa | |
Zugfestigkeit | 23.0 °C | 440 MPa Show Material materials with Zugfestigkeit of 440 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.4E-5 1/K | Typical for Malleable Cast Iron |
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Malleable Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 51 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 51 W/(m·K) | Typical for Malleable Cast Iron |