Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.6 - 2.7 g/cm³ Show Material materials with Dichte of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 12.0 % Show Material materials with Dehnung of 12.0 % | as-cast | JIS H5202 | Casting | |
Elastizitätsmodul | 68.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Zugfestigkeit | 216.0 MPa Show Material materials with Zugfestigkeit of 216.0 MPa | as-cast | JIS H5202 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Schmelzpunkt | 450.0 - 640.0 °C Show Material materials with Schmelzpunkt of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Wärmeleitfähigkeit | 60.0 - 140.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |