Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % |
Flächenreduzierung | 20.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 214 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 214 MPa |
Zugfestigkeit | 20.0 °C | 500 MPa Show Material materials with Zugfestigkeit of 500 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 26 - 28 % Show Material materials with Chrom of 26 - 28 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.6 - 1.4 % Show Material materials with Kupfer of 0.6 - 1.4 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 4 - 5 % Show Material materials with Molybdän of 4 - 5 % |
Nickel | 30 - 34 % Show Material materials with Nickel of 30 - 34 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |