Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 2 - 3 % Show Material materials with Chrom of 2 - 3 % |
Kobalt | 0.5 % Show Material materials with Kobalt of 0.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 4 - 6 % Show Material materials with Kupfer of 4 - 6 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 75 - 78 % Show Material materials with Nickel of 75 - 78 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |