Mechanisch
Property | Temperature | Value |
---|---|---|
Zugfestigkeit | 20.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 10 - 14 % Show Material materials with Chrom of 10 - 14 % |
Kohlenstoff | 0.35 - 0.75 % Show Material materials with Kohlenstoff of 0.35 - 0.75 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 58 - 62 % Show Material materials with Nickel of 58 - 62 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 2.5 % Show Material materials with Silizium of 2.5 % |