Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.75 - 8.4 g/cm³ Show Material materials with Dichte of 7.75 - 8.4 g/cm³ | Typical for Nickel Chromium Iron Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 4.5 % Show Material materials with Dehnung A50 of 4.5 % | |
Elastizitätsmodul | 23.0 °C | 150 GPa Show Material materials with Elastizitätsmodul of 150 GPa | Typical for Nickel Chromium Iron Alloy |
Streckgrenze | 23.0 °C | 235 MPa Show Material materials with Streckgrenze of 235 MPa | |
Zugfestigkeit | 23.0 °C | 430 MPa Show Material materials with Zugfestigkeit of 430 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Iron Alloy |
Schmelzpunkt | 1200 - 1480 °C Show Material materials with Schmelzpunkt of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Iron Alloy |
Wärmeleitfähigkeit | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8 - 35 W/(m·K) | Typical for Nickel Chromium Iron Alloy |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 28 % Show Material materials with Chrom of 24 - 28 % |
Kohlenstoff | 0.35 - 0.75 % Show Material materials with Kohlenstoff of 0.35 - 0.75 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 33 - 37 % Show Material materials with Nickel of 33 - 37 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 2.5 % Show Material materials with Silizium of 2.5 % |