Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 23.0 °C | 131 - 183 [-] Show Material materials with Härte, Brinell of 131 - 183 [-] |
Zugfestigkeit | 23.0 °C | 172 MPa Show Material materials with Zugfestigkeit of 172 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1.5 - 2.5 % Show Material materials with Chrom of 1.5 - 2.5 % |
Kohlenstoff | 3 % Show Material materials with Kohlenstoff of 3 % |
Kupfer | 5.5 - 7.5 % Show Material materials with Kupfer of 5.5 - 7.5 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 13.5 - 17.5 % Show Material materials with Nickel of 13.5 - 17.5 % |
Schwefel | 0.12 % Show Material materials with Schwefel of 0.12 % |
Silizium | 1 - 2.8 % Show Material materials with Silizium of 1 - 2.8 % |