Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.15 g/cm³ Show Material materials with Dichte of 7.15 g/cm³ | Typical for Grey Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 92.4 GPa Show Material materials with Elastizitätsmodul of 92.4 GPa | Typical for Grey Cast Iron |
Härte, Brinell | 23.0 °C | 124 - 174 [-] Show Material materials with Härte, Brinell of 124 - 174 [-] | |
Poissonzahl | 23.0 °C | 0.21 [-] Show Material materials with Poissonzahl of 0.21 [-] | Typical for Grey Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Zugfestigkeit | 23.0 °C | 172 MPa Show Material materials with Zugfestigkeit of 172 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.5E-5 1/K | Typical for Grey Cast Iron |
Schmelzpunkt | 1127 - 1204 °C Show Material materials with Schmelzpunkt of 1127 - 1204 °C | Typical for Grey Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Grey Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 20 - 80 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 20 - 80 W/(m·K) | Typical for Grey Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 1 - 2 % Show Material materials with Chrom of 1 - 2 % |
Kohlenstoff | 3 % Show Material materials with Kohlenstoff of 3 % |
Kupfer | 3.5 - 5.5 % Show Material materials with Kupfer of 3.5 - 5.5 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Molybdän | 1 % Show Material materials with Molybdän of 1 % |
Nickel | 18 - 22 % Show Material materials with Nickel of 18 - 22 % |
Schwefel | 0.12 % Show Material materials with Schwefel of 0.12 % |
Silizium | 1.5 - 2.5 % Show Material materials with Silizium of 1.5 - 2.5 % |