Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % |
Härte, Brinell | 20.0 °C | 131 - 193 [-] Show Material materials with Härte, Brinell of 131 - 193 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 210 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 210 MPa |
Zugfestigkeit | 20.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1.75 - 2.25 % Show Material materials with Chrom of 1.75 - 2.25 % |
Kohlenstoff | 2.3 % Show Material materials with Kohlenstoff of 2.3 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 34 - 37 % Show Material materials with Nickel of 34 - 37 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Silizium | 4.9 - 5.5 % Show Material materials with Silizium of 4.9 - 5.5 % |