Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 23 - 28 % Show Material materials with Chrom of 23 - 28 % |
Kohlenstoff | 0.2 - 0.45 % Show Material materials with Kohlenstoff of 0.2 - 0.45 % |
Mangan | 2.5 % Show Material materials with Mangan of 2.5 % |
Nickel | 10 - 14 % Show Material materials with Nickel of 10 - 14 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1.75 % Show Material materials with Silizium of 1.75 % |
Stickstoff | 0.2 % Show Material materials with Stickstoff of 0.2 % |