Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 11 - 14 % Show Material materials with Chrom of 11 - 14 % |
Kohlenstoff | 2 - 3.3 % Show Material materials with Kohlenstoff of 2 - 3.3 % |
Kupfer | 1.2 % Show Material materials with Kupfer of 1.2 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 3 % Show Material materials with Molybdän of 3 % |
Nickel | 2.5 % Show Material materials with Nickel of 2.5 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Schwefel | 0.06 % Show Material materials with Schwefel of 0.06 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |