Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Dichte of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa | Typical for Cast Iron |
Härte, Brinell | 23.0 °C | 400 [-] Show Material materials with Härte, Brinell of 400 [-] | |
Härte, Rockwell C | 23.0 °C | 41 [-] Show Material materials with Härte, Rockwell C of 41 [-] | |
Härte, Vickers | 23.0 °C | 430 [-] Show Material materials with Härte, Vickers of 430 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 14 - 18 % Show Material materials with Chrom of 14 - 18 % |
Kohlenstoff | 2 - 3.3 % Show Material materials with Kohlenstoff of 2 - 3.3 % |
Kupfer | 1.2 % Show Material materials with Kupfer of 1.2 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 3 % Show Material materials with Molybdän of 3 % |
Nickel | 2.5 % Show Material materials with Nickel of 2.5 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Schwefel | 0.06 % Show Material materials with Schwefel of 0.06 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |