Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % |
Flächenreduzierung | 23.0 °C | 18 % Show Material materials with Flächenreduzierung of 18 % |
Härte, Brinell | 23.0 °C | 248 - 341 [-] Show Material materials with Härte, Brinell of 248 - 341 [-] |
Härte, Rockwell C | 23.0 °C | 24 - 37 [-] Show Material materials with Härte, Rockwell C of 24 - 37 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 585 MPa Show Material materials with Streckgrenze Rp 0,2 of 585 MPa |
Zugfestigkeit | 23.0 °C | 895 MPa Show Material materials with Zugfestigkeit of 895 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 18 - 21 % Show Material materials with Chrom of 18 - 21 % |
Kohlenstoff | 0.28 - 0.35 % Show Material materials with Kohlenstoff of 0.28 - 0.35 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 0.75 - 1.5 % Show Material materials with Mangan of 0.75 - 1.5 % |
Molybdän | 1 - 1.75 % Show Material materials with Molybdän of 1 - 1.75 % |
Nickel | 8 - 11 % Show Material materials with Nickel of 8 - 11 % |
Niobium | 0.25 - 0.6 % Show Material materials with Niobium of 0.25 - 0.6 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.3 - 0.8 % Show Material materials with Silizium of 0.3 - 0.8 % |
Titan | 0.1 - 0.35 % Show Material materials with Titan of 0.1 - 0.35 % |
Wolfram | 1 - 1.75 % Show Material materials with Wolfram of 1 - 1.75 % |