Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 12 % Show Material materials with Dehnung A50 of 12 % |
Flächenreduzierung | 23.0 °C | 15 % Show Material materials with Flächenreduzierung of 15 % |
Härte, Brinell | 23.0 °C | 311 - 388 [-] Show Material materials with Härte, Brinell of 311 - 388 [-] |
Härte, Rockwell C | 23.0 °C | 32 - 41 [-] Show Material materials with Härte, Rockwell C of 32 - 41 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 830 MPa Show Material materials with Streckgrenze Rp 0,2 of 830 MPa |
Zugfestigkeit | 23.0 °C | 1170 MPa Show Material materials with Zugfestigkeit of 1170 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Bor | 0.01 - 0.07 % Show Material materials with Bor of 0.01 - 0.07 % |
Chrom | 12 - 15 % Show Material materials with Chrom of 12 - 15 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % |
Mangan | 1.25 - 2 % Show Material materials with Mangan of 1.25 - 2 % |
Molybdän | 1.25 - 2.25 % Show Material materials with Molybdän of 1.25 - 2.25 % |
Nickel | 24 - 28 % Show Material materials with Nickel of 24 - 28 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.1 - 0.8 % Show Material materials with Silizium of 0.1 - 0.8 % |
Titan | 2.7 - 3.3 % Show Material materials with Titan of 2.7 - 3.3 % |