Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % |
Flächenreduzierung | 23.0 °C | 18 % Show Material materials with Flächenreduzierung of 18 % |
Härte, Brinell | 23.0 °C | 248 [-] Show Material materials with Härte, Brinell of 248 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 585 MPa Show Material materials with Streckgrenze Rp 0,2 of 585 MPa |
Zugfestigkeit | 23.0 °C | 895 MPa Show Material materials with Zugfestigkeit of 895 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.35 % Show Material materials with Aluminium of 0.35 % |
Bor | 0.001 - 0.01 % Show Material materials with Bor of 0.001 - 0.01 % |
Chrom | 13.5 - 16 % Show Material materials with Chrom of 13.5 - 16 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 1 - 1.5 % Show Material materials with Molybdän of 1 - 1.5 % |
Nickel | 24 - 27 % Show Material materials with Nickel of 24 - 27 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 1.9 - 2.35 % Show Material materials with Titan of 1.9 - 2.35 % |
Vanadium | 0.1 - 0.5 % Show Material materials with Vanadium of 0.1 - 0.5 % |