Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Dichte of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 25 % Show Material materials with Dehnung of 25 % | |
Elastizitätsmodul | 23.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa | Typical for Cast Iron |
Härte, Brinell | 23.0 °C | 111 - 171 [-] Show Material materials with Härte, Brinell of 111 - 171 [-] | |
Kerbschlagenergie | 23.0 °C | 27 J Show Material materials with Kerbschlagenergie of 27 J | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Streckgrenze Rp 0,2 | 23.0 °C | 170 MPa Show Material materials with Streckgrenze Rp 0,2 of 170 MPa | |
Zugfestigkeit | 23.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 0.2 % Show Material materials with Chrom of 0.2 % |
Kohlenstoff | 2.2 - 2.7 % Show Material materials with Kohlenstoff of 2.2 - 2.7 % |
Mangan | 3.75 - 4.5 % Show Material materials with Mangan of 3.75 - 4.5 % |
Nickel | 21 - 24 % Show Material materials with Nickel of 21 - 24 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Silizium | 1.5 - 2.5 % Show Material materials with Silizium of 1.5 - 2.5 % |