Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.77 g/cm³ Show Material materials with Dichte of 7.6 - 7.77 g/cm³ | Typical for White Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 165 - 240 GPa Show Material materials with Elastizitätsmodul of 165 - 240 GPa | Typical for White Cast Iron |
Härte, Vickers | 20.0 °C | 350 [-] Show Material materials with Härte, Vickers of 350 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | Typical for White Cast Iron |
Schmelzpunkt | 1209 °C Show Material materials with Schmelzpunkt of 1209 °C | Typical for White Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for White Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 22 - 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 22 - 30 W/(m·K) | Typical for White Cast Iron |
Chemical properties
Property | Value |
---|---|
Chrom | 2 % Show Material materials with Chrom of 2 % |
Kohlenstoff | 2.4 - 3.9 % Show Material materials with Kohlenstoff of 2.4 - 3.9 % |
Mangan | 0.2 - 1 % Show Material materials with Mangan of 0.2 - 1 % |
Silizium | 0.4 - 1.5 % Show Material materials with Silizium of 0.4 - 1.5 % |