Property | Value |
---|---|
Chrom | 19 - 22 % Show Material materials with Chrom of 19 - 22 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Kupfer | 3 - 4 % Show Material materials with Kupfer of 3 - 4 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 2 - 3 % Show Material materials with Molybdän of 2 - 3 % |
Nickel | 27.5 - 30.5 % Show Material materials with Nickel of 27.5 - 30.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |