Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 4.506 g/cm³ Show Material materials with Dichte of 4.506 g/cm³ | Typical for Pure Titanium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 23.0 % Show Material materials with Dehnung of 23.0 % | Hot-Extruded | JIS H4630 | Tube, Pipe | |
Elastizitätsmodul | 120.0 GPa Show Material materials with Elastizitätsmodul of 120.0 GPa | Typical for Pure Titanium | |||
Poissonzahl | 0.361 [-] Show Material materials with Poissonzahl of 0.361 [-] | Typical for Pure Titanium | |||
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Typical for Pure Titanium | |||
Zugfestigkeit | 343.0 MPa Show Material materials with Zugfestigkeit of 343.0 MPa | Hot-Extruded | JIS H4630 | Tube, Pipe |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium |
Schmelzpunkt | 1670.0 °C Show Material materials with Schmelzpunkt of 1670.0 °C | Typical for Pure Titanium |
Spezifische Wärmekapazität | 513.0 - 599.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 513.0 - 599.0 J/(kg·K) | Typical for Pure Titanium |
Wärmeleitfähigkeit | 15.0 - 22.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15.0 - 22.0 W/(m·K) | Typical for Pure Titanium |
Technological properties
Property | ||
---|---|---|
Processing history | hot extruded |