Mechanisch
Chemical properties
Property | Value |
---|---|
Eisen | 3.5 % Show Material materials with Eisen of 3.5 % |
Kohlenstoff | 0.35 % Show Material materials with Kohlenstoff of 0.35 % |
Kupfer | 26 - 33 % Show Material materials with Kupfer of 26 - 33 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Niobium | 0.5 % Show Material materials with Niobium of 0.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 2 % Show Material materials with Silizium of 2 % |