Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 195 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 195 MPa |
Zugfestigkeit | 20.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 13 - 17 % Show Material materials with Chrom of 13 - 17 % |
Kohlenstoff | 0.25 - 0.35 % Show Material materials with Kohlenstoff of 0.25 - 0.35 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 33 - 37 % Show Material materials with Nickel of 33 - 37 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 2.5 % Show Material materials with Silizium of 2.5 % |