Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 17.5 % Show Material materials with Chrom of 15 - 17.5 % |
Eisen | 2 % Show Material materials with Eisen of 2 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 15 - 17.5 % Show Material materials with Molybdän of 15 - 17.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Wolfram | 1 % Show Material materials with Wolfram of 1 % |