Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 19 - 22 % Show Material materials with Chrom of 19 - 22 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 3 - 3.5 % Show Material materials with Kupfer of 3 - 3.5 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 2 - 3 % Show Material materials with Molybdän of 2 - 3 % |
Nickel | 27.5 - 30.5 % Show Material materials with Nickel of 27.5 - 30.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |