Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % |
Flächenreduzierung | 20.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 240 MPa |
Zugfestigkeit | 20.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 20.5 - 23.5 % Show Material materials with Chrom of 20.5 - 23.5 % |
Kohlenstoff | 0.06 % Show Material materials with Kohlenstoff of 0.06 % |
Mangan | 4 - 6 % Show Material materials with Mangan of 4 - 6 % |
Molybdän | 1.5 - 3 % Show Material materials with Molybdän of 1.5 - 3 % |
Nickel | 11.5 - 13.5 % Show Material materials with Nickel of 11.5 - 13.5 % |
Niobium | 0.1 - 0.3 % Show Material materials with Niobium of 0.1 - 0.3 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |