Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 2 - 3 % Show Material materials with Molybdän of 2 - 3 % |
Nickel | 32 - 38 % Show Material materials with Nickel of 32 - 38 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |