Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 18 % Show Material materials with Dehnung of 18 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 549 MPa Show Material materials with Streckgrenze of 549 MPa | |
Zugfestigkeit | 23.0 °C | 686 MPa Show Material materials with Zugfestigkeit of 686 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | quenched and tempered |