Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 35 % Show Material materials with Dehnung of 35 % |
Dehnung, transversal | 20.0 °C | 35 % Show Material materials with Dehnung, transversal of 35 % |
Elastizitätsmodul | -253.0 °C | 161 GPa Show Material materials with Elastizitätsmodul of 161 GPa |
-195.0 °C | 158 GPa Show Material materials with Elastizitätsmodul of 158 GPa | |
-100.0 °C | 155 GPa Show Material materials with Elastizitätsmodul of 155 GPa | |
20.0 °C | 150 GPa Show Material materials with Elastizitätsmodul of 150 GPa | |
50.0 °C | 150 GPa Show Material materials with Elastizitätsmodul of 150 GPa | |
100.0 °C | 149 GPa Show Material materials with Elastizitätsmodul of 149 GPa | |
150.0 °C | 148 GPa Show Material materials with Elastizitätsmodul of 148 GPa | |
200.0 °C | 146 GPa Show Material materials with Elastizitätsmodul of 146 GPa | |
250.0 °C | 144 GPa Show Material materials with Elastizitätsmodul of 144 GPa | |
300.0 °C | 142 GPa Show Material materials with Elastizitätsmodul of 142 GPa | |
350.0 °C | 141 GPa Show Material materials with Elastizitätsmodul of 141 GPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa |
Streckgrenze Rp 0,2, transversal | 20.0 °C | 150 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 150 MPa |
Streckgrenze Rp 1,0 | 50.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 1,0 of 175 MPa |
100.0 °C | 163 MPa Show Material materials with Streckgrenze Rp 1,0 of 163 MPa | |
150.0 °C | 158 MPa Show Material materials with Streckgrenze Rp 1,0 of 158 MPa | |
200.0 °C | 153 MPa Show Material materials with Streckgrenze Rp 1,0 of 153 MPa | |
250.0 °C | 148 MPa Show Material materials with Streckgrenze Rp 1,0 of 148 MPa | |
300.0 °C | 143 MPa Show Material materials with Streckgrenze Rp 1,0 of 143 MPa | |
350.0 °C | 138 MPa Show Material materials with Streckgrenze Rp 1,0 of 138 MPa | |
Streckgrenze Rp 1,0, transversal | 20.0 °C | 140 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 140 MPa |
50.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 175 MPa | |
100.0 °C | 163 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 163 MPa | |
150.0 °C | 148 - 158 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 148 - 158 MPa | |
200.0 °C | 138 - 153 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 138 - 153 MPa | |
250.0 °C | 148 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 148 MPa | |
300.0 °C | 143 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 143 MPa | |
350.0 °C | 138 MPa Show Material materials with Streckgrenze Rp 1,0, transversal of 138 MPa | |
Zugfestigkeit | 20.0 °C | 350 - 420 MPa Show Material materials with Zugfestigkeit of 350 - 420 MPa |
Zugfestigkeit, transversal | 20.0 °C | 350 MPa Show Material materials with Zugfestigkeit, transversal of 350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 20.0 °C | 29 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 29 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.4 - 1 % Show Material materials with Eisen of 0.4 - 1 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 30 - 32 % Show Material materials with Nickel of 30 - 32 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |