Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.85 - 8.9 g/cm³ Show Material materials with Dichte of 8.85 - 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 55 % Show Material materials with Dehnung of 55 % |
Dehnung A50 | 20.0 °C | 45 % Show Material materials with Dehnung A50 of 45 % |
Elastizitätsmodul | 20.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa |
Härte, Vickers | 20.0 °C | 75 - 105 [-] Show Material materials with Härte, Vickers of 75 - 105 [-] |
Poissonzahl | 20.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 20.0 °C | 310 - 390 MPa Show Material materials with Zugfestigkeit of 310 - 390 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 20.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 96 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 96 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.00E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.00E+7 S/m |
Specific Electrical conductivity | 17 % IACS Show Material materials with Specific Electrical conductivity of 17 % IACS |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.01 - 0.4 % Show Material materials with Phosphor of 0.01 - 0.4 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |