Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 45 % Show Material materials with Dehnung of 45 % | |
Elastizitätsmodul | 23.0 °C | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze |
Elongation A10 | 20.0 °C | 40 % Show Material materials with Elongation A10 of 40 % | |
Elongation A100 | 20.0 °C | 35 % Show Material materials with Elongation A100 of 35 % | |
Elongation A11.3 | 20.0 °C | 40 % Show Material materials with Elongation A11.3 of 40 % | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze |
Streckgrenze Rp 0,2 | 20.0 °C | 260 - 280 MPa Show Material materials with Streckgrenze Rp 0,2 of 260 - 280 MPa | |
Zugfestigkeit | 20.0 °C | 390 MPa Show Material materials with Zugfestigkeit of 390 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Spezifische Wärmekapazität | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Phosphor | 0.2 - 0.4 % Show Material materials with Phosphor of 0.2 - 0.4 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 7.5 - 8.5 % Show Material materials with Zinn of 7.5 - 8.5 % |