Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 2 - 15 % Show Material materials with Dehnung of 2 - 15 % |
Dehnung A50 | 20.0 °C | 2 - 16 % Show Material materials with Dehnung A50 of 2 - 16 % |
Elastizitätsmodul | 20.0 °C | 135 GPa Show Material materials with Elastizitätsmodul of 135 GPa |
Elongation A10 | 20.0 °C | 6 - 8 % Show Material materials with Elongation A10 of 6 - 8 % |
Elongation A100 | 20.0 °C | 5 - 10 % Show Material materials with Elongation A100 of 5 - 10 % |
Härte, Brinell | 20.0 °C | 155 - 350 [-] Show Material materials with Härte, Brinell of 155 - 350 [-] |
Härte, Vickers | 20.0 °C | 120 - 450 [-] Show Material materials with Härte, Vickers of 120 - 450 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 450 - 1420 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 - 1420 MPa |
Zugfestigkeit | 20.0 °C | 510 - 1520 MPa Show Material materials with Zugfestigkeit of 510 - 1520 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Wärmeleitfähigkeit | 20.0 °C | 92 - 125 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 92 - 125 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 8.00E+6 - 1.80E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 8.00E+6 - 1.80E+7 S/m |
Specific Electrical conductivity | 23 % IACS Show Material materials with Specific Electrical conductivity of 23 % IACS |
Chemical properties
Property | Value |
---|---|
Beryllium | 1.8 - 2.1 % Show Material materials with Beryllium of 1.8 - 2.1 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kobalt | 0.3 % Show Material materials with Kobalt of 0.3 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |