Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 - 8.8 g/cm³ Show Material materials with Dichte of 8.3 - 8.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 8 % Show Material materials with Dehnung of 8 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Elongation A100 | 20.0 °C | 2 - 4 % Show Material materials with Elongation A100 of 2 - 4 % | |
Elongation A11.3 | 20.0 °C | 4 - 6 % Show Material materials with Elongation A11.3 of 4 - 6 % | |
Streckgrenze Rp 0,2 | 20.0 °C | 610 MPa Show Material materials with Streckgrenze Rp 0,2 of 610 MPa | |
Zugfestigkeit | 20.0 °C | 730 MPa Show Material materials with Zugfestigkeit of 730 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 2.80E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 2.80E+7 S/m |
Specific Electrical conductivity | 48 % IACS Show Material materials with Specific Electrical conductivity of 48 % IACS |
Chemical properties
Property | Value |
---|---|
Beryllium | 0.4 - 0.7 % Show Material materials with Beryllium of 0.4 - 0.7 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kobalt | 0.8 - 1.3 % Show Material materials with Kobalt of 0.8 - 1.3 % |
Nickel | 0.8 - 1.3 % Show Material materials with Nickel of 0.8 - 1.3 % |