Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 10 % Show Material materials with Dehnung of 10 % |
Elongation A100 | 20.0 °C | 6 % Show Material materials with Elongation A100 of 6 % |
Härte, Vickers | 20.0 °C | 230 [-] Show Material materials with Härte, Vickers of 230 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 760 MPa Show Material materials with Streckgrenze Rp 0,2 of 760 MPa |
Zugfestigkeit | 20.0 °C | 750 - 950 MPa Show Material materials with Zugfestigkeit of 750 - 950 MPa |
Chemical properties
Property | Value |
---|---|
Beryllium | 0.4 - 0.7 % Show Material materials with Beryllium of 0.4 - 0.7 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kobalt | 0.8 - 1.3 % Show Material materials with Kobalt of 0.8 - 1.3 % |
Nickel | 0.8 - 1.3 % Show Material materials with Nickel of 0.8 - 1.3 % |