Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.92 g/cm³ Show Material materials with Dichte of 8.92 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Härte, Brinell | 20.0 °C | 190 [-] Show Material materials with Härte, Brinell of 190 [-] | |
Härte, Vickers | 20.0 °C | 200 [-] Show Material materials with Härte, Vickers of 200 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 500 MPa Show Material materials with Streckgrenze Rp 0,2 of 500 MPa | |
Zugfestigkeit | 20.0 °C | 650 MPa Show Material materials with Zugfestigkeit of 650 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.77E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.77E-5 1/K | |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 20.0 °C | 385 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 385 J/(kg·K) |
Chemical properties
Property | Value |
---|---|
Nickel | 0.8 - 1.2 % Show Material materials with Nickel of 0.8 - 1.2 % |
Phosphor | 0.15 - 0.25 % Show Material materials with Phosphor of 0.15 - 0.25 % |