Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Härte, Brinell | 20.0 °C | 105 [-] Show Material materials with Härte, Brinell of 105 [-] | |
Härte, Vickers | 20.0 °C | 110 [-] Show Material materials with Härte, Vickers of 110 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 250 - 300 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 - 300 MPa | |
Zugfestigkeit | 20.0 °C | 360 - 370 MPa Show Material materials with Zugfestigkeit of 360 - 370 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 - 1.2 % Show Material materials with Chrom of 0.5 - 1.2 % |
Eisen | 0.08 % Show Material materials with Eisen of 0.08 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |