CuCr1Zr, mat. No CW106C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuCrZr, mat. No 2.1293, acc. to DIN 17666 : 1983-12 applies: The strength values of CuCrZr are more favorable than of CuCr especially at higher temperatures. CuCrZr shows the following properties: high strength at room temperature, high temperature for removal of workhardening, high creep strength, no notch sensitivity at increased temperatures. Temperature for removal of workhardening approximates 500°C. Favorable electrical and thermal conductivity. Processing properties: hot and cold forming: good machinability: moderately soft soldering: moderately hard soldering: moderately gas shielded welding: moderately burnishing: good Application: For live springs and contacts, electrodes for resistance welding.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.8 - 8.92 g/cm³

Show Material materials with Dichte of 8.8 - 8.92 g/cm³

Mechanisch

PropertyTemperatureValue

Dehnung

20.0 °C

8 %

Show Material materials with Dehnung of 8 %

Elastizitätsmodul

20.0 °C

130 GPa

Show Material materials with Elastizitätsmodul of 130 GPa

Elongation A100

20.0 °C

2 - 3 %

Show Material materials with Elongation A100 of 2 - 3 %

Elongation A11.3

20.0 °C

5 - 6 %

Show Material materials with Elongation A11.3 of 5 - 6 %

Streckgrenze Rp 0,2

20.0 °C

420 MPa

Show Material materials with Streckgrenze Rp 0,2 of 420 MPa

Zugfestigkeit

20.0 °C

470 MPa

Show Material materials with Zugfestigkeit of 470 MPa

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

100.0 °C

1.63E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.63E-5 1/K

200.0 °C

1.7E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K

300.0 °C

1.76E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.76E-5 1/K

Schmelzpunkt

855 - 1090 °C

Show Material materials with Schmelzpunkt of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Spezifische Wärmekapazität

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Wärmeleitfähigkeit

20.0 °C

320 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 320 W/(m·K)

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

4.30E+7 - 4.60E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 4.30E+7 - 4.60E+7 S/m

Specific Electrical conductivity

74 - 79 % IACS

Show Material materials with Specific Electrical conductivity of 74 - 79 % IACS

Chemical properties

PropertyValue

Chrom

0.5 - 1.2 %

Show Material materials with Chrom of 0.5 - 1.2 %

Eisen

0.08 %

Show Material materials with Eisen of 0.08 %

Silizium

0.1 %

Show Material materials with Silizium of 0.1 %

Zirkonium

0.03 - 0.3 %

Show Material materials with Zirkonium of 0.03 - 0.3 %