Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 - 8.91 g/cm³ Show Material materials with Dichte of 8.9 - 8.91 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 8 - 15 % Show Material materials with Dehnung of 8 - 15 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Elongation A10 | 20.0 °C | 7 - 13 % Show Material materials with Elongation A10 of 7 - 13 % | |
Elongation A100 | 20.0 °C | 11 % Show Material materials with Elongation A100 of 11 % | |
Härte, Brinell | 20.0 °C | 120 - 180 [-] Show Material materials with Härte, Brinell of 120 - 180 [-] | |
Härte, Vickers | 20.0 °C | 125 - 185 [-] Show Material materials with Härte, Vickers of 125 - 185 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 270 - 380 MPa Show Material materials with Streckgrenze Rp 0,2 of 270 - 380 MPa | |
Zugfestigkeit | 20.0 °C | 360 - 470 MPa Show Material materials with Zugfestigkeit of 360 - 470 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.63E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.63E-5 1/K | |
200.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | ||
300.0 °C | 1.76E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.76E-5 1/K | ||
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 - 1.2 % Show Material materials with Chrom of 0.5 - 1.2 % |
Eisen | 0.08 % Show Material materials with Eisen of 0.08 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zirkonium | 0.03 - 0.3 % Show Material materials with Zirkonium of 0.03 - 0.3 % |