Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 14 % Show Material materials with Dehnung of 14 % |
Elastizitätsmodul | 20.0 °C | 150 GPa Show Material materials with Elastizitätsmodul of 150 GPa |
Elongation A10 | 20.0 °C | 12 % Show Material materials with Elongation A10 of 12 % |
Elongation A100 | 20.0 °C | 10 % Show Material materials with Elongation A100 of 10 % |
Elongation A11.3 | 20.0 °C | 12 % Show Material materials with Elongation A11.3 of 12 % |
Streckgrenze Rp 0,2 | 20.0 °C | 180 MPa Show Material materials with Streckgrenze Rp 0,2 of 180 MPa |
Zugfestigkeit | 20.0 °C | 420 MPa Show Material materials with Zugfestigkeit of 420 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 20.0 °C | 29 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 29 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.4 - 1 % Show Material materials with Eisen of 0.4 - 1 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 30 - 32 % Show Material materials with Nickel of 30 - 32 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |