Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 5 % Show Material materials with Dehnung of 5 % |
Elastizitätsmodul | 20.0 °C | 115 GPa Show Material materials with Elastizitätsmodul of 115 GPa |
Elongation A10 | 20.0 °C | 3 % Show Material materials with Elongation A10 of 3 % |
Elongation A100 | 20.0 °C | 2 % Show Material materials with Elongation A100 of 2 % |
Elongation A11.3 | 20.0 °C | 3 % Show Material materials with Elongation A11.3 of 3 % |
Härte, Brinell | 20.0 °C | 95 - 130 [-] Show Material materials with Härte, Brinell of 95 - 130 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 240 - 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 240 - 250 MPa |
Zugfestigkeit | 20.0 °C | 300 MPa Show Material materials with Zugfestigkeit of 300 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Wärmeleitfähigkeit | 20.0 °C | 350 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 350 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.00E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.00E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Property | Value |
---|---|
Blei | 0.7 - 1.5 % Show Material materials with Blei of 0.7 - 1.5 % |
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |