Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 20 - 25 % Show Material materials with Dehnung of 20 - 25 % |
Elastizitätsmodul | 20.0 °C | 102 GPa Show Material materials with Elastizitätsmodul of 102 GPa |
Elongation A100 | 20.0 °C | 10 % Show Material materials with Elongation A100 of 10 % |
Elongation A11.3 | 20.0 °C | 15 % Show Material materials with Elongation A11.3 of 15 % |
Schubmodule | 20.0 °C | 37 GPa Show Material materials with Schubmodule of 37 GPa |
Streckgrenze Rp 0,2 | 20.0 °C | 150 - 300 MPa Show Material materials with Streckgrenze Rp 0,2 of 150 - 300 MPa |
Zugfestigkeit | 20.0 °C | 360 MPa Show Material materials with Zugfestigkeit of 360 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 2.04E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.04E-5 1/K | |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 20.0 °C | 109 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 109 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.39E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.39E+7 S/m |
spezifischer Widerstand | 20.0 °C | 7.2E-8 Ω·m Show Material materials with spezifischer Widerstand of 7.2E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 0.2 - 0.8 % Show Material materials with Blei of 0.2 - 0.8 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 59 - 60.5 % Show Material materials with Kupfer of 59 - 60.5 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |